低水泥高铝浇注料 · Service temperature ≤1400℃ · Indicative price 区间询价

Core Specifications

MaterialHigh alumina (Al₂O₃ ≥ 60%)
Max service temp1400°C
CCS (110°C×24h)60 MPa
Linear change±0.3% (1350°C×3h)
Bonding systemLow cement
InstallationVibration / self-flow

Recommended Zones

Ladle permanent lining
Tundish permanent lining
Reheating furnace lining
Iron runner

More zone solutions: Application Solutions

Procurement Info

MOQ1 ton (small batches negotiable)
Standard lead time7-15 days
Packing25 kg bags / pallets; export wooden cases optional
SamplesAvailable for testing before bulk order
InvoicingVAT invoice available

FAQ

Q: What to watch during low cement castable installation?

A: Strictly control water addition per the datasheet, mix 3-5 minutes, cast in one pass, cure then follow the heating curve for drying.

Q: Low cement vs regular castable?

A: Low cement castable uses microsilica plus a small amount of CAC for bonding: higher hot strength and lower porosity, preferred for medium-high temperature zones.